Extrudr XPETG CF vs ASA

Compare Extrudr XPETG CF and ASA filaments side-by-side so you can pick the right one for your 3D printing project.

Extrudr XPETG CF vs ASA: Extrudr XPETG CF is known for tougher than pla, while ASA is known for excellent uv resistance (outdoors indefinitely). Extrudr XPETG CF is easier to print; ASA prints at higher nozzle temperatures (220-275°C vs 235°C). Choose Extrudr XPETG CF for tougher than pla, or ASA for excellent uv resistance (outdoors indefinitely).

Key differences at a glance

Property
Extrudr XPETG CF
ASA
Nozzle temp
235°C
220-275°C
Bed temp
70°C
90-110°C
Enclosure needed
No
Recommended
Ease of printing
Easy
Moderate
Moisture sensitivity
low
moderate

Detailed Comparison

Property
Extrudr XPETG CF
ASA
Tier Rating
Tier null
Tier A
Family
PETG
ASA
Nozzle Temp
235°C
220-275°C
Bed Temp
70°C
90-110°C
Enclosure
not needed
recommended
Cooling
Low to moderate; avoid drafts
Moisture Sensitivity
low
moderate

Green marks the generally easier or more forgiving option in that row, based on tier, enclosure needs, and moisture sensitivity. It is not always the better choice for a specific job, so weigh it against what your project actually needs.

Strengths Comparison

Extrudr XPETG CF Strengths

  • Tougher than PLA, higher temp tolerance, more durable in real-world use
  • Good clarity and low friction among easy-to-print materials

ASA Strengths

  • Excellent UV resistance (outdoors indefinitely), tough, matte surface
  • Less warping than ABS; low viscosity enables very high speed printing
  • High heat tolerance (~boiling water range)

Considerations

Extrudr XPETG CF Caveats

  • Overhangs/bridges sag; supports can be hard to remove
  • Absorbs water fairly quickly

ASA Caveats

  • Still off-gasses; enclosure/ventilation recommended
  • Can still warp; needs tuning

Frequently Asked Questions

What is the difference between Extrudr XPETG CF and ASA?
Extrudr XPETG CF prints at 235°C nozzle / 70°C bed (No enclosure, low moisture sensitivity). ASA prints at 220-275°C nozzle / 90-110°C bed (Recommended enclosure, moderate moisture sensitivity).
Is Extrudr XPETG CF or ASA stronger?
Our dataset does not include comparable tensile strength values for both. Qualitatively, Extrudr XPETG CF is suited to tougher than pla, while ASA is suited to excellent uv resistance (outdoors indefinitely).
Which prints at a higher temperature, Extrudr XPETG CF or ASA?
ASA prints at a higher temperature (220-275°C nozzle vs 235°C for Extrudr XPETG CF).
Is Extrudr XPETG CF or ASA better for beginners?
Extrudr XPETG CF is better for beginners: enclosure is no and moisture sensitivity is low, vs recommended enclosure and moderate moisture for ASA.
Should I use Extrudr XPETG CF or ASA for outdoor use?
For outdoor use, ASA is usually the better fit (Excellent UV resistance (outdoors indefinitely)). Choose Extrudr XPETG CF instead when tougher than pla.

Other Popular Comparisons