Fillamentum CPE vs ASA

Compare Fillamentum CPE and ASA filaments side-by-side so you can pick the right one for your 3D printing project.

Fillamentum CPE vs ASA: Fillamentum CPE is known for better chemical resistance than petg, while ASA is known for excellent uv resistance (outdoors indefinitely). Fillamentum CPE is easier to print; Fillamentum CPE prints at higher nozzle temperatures (275°C vs 220-275°C). Choose Fillamentum CPE for better chemical resistance than petg, or ASA for excellent uv resistance (outdoors indefinitely).

Key differences at a glance

Property
Fillamentum CPE
ASA
Nozzle temp
275°C
220-275°C
Bed temp
90°C
90-110°C
Enclosure needed
No
Recommended
Ease of printing
Easy
Moderate
Moisture sensitivity
low
moderate

Detailed Comparison

Property
Fillamentum CPE
ASA
Tier Rating
Tier null
Tier A
Family
CPE
ASA
Nozzle Temp
275°C
220-275°C
Bed Temp
90°C
90-110°C
Enclosure
not needed
recommended
Cooling
Low to moderate; avoid drafts
Moisture Sensitivity
low
moderate

Green marks the generally easier or more forgiving option in that row, based on tier, enclosure needs, and moisture sensitivity. It is not always the better choice for a specific job, so weigh it against what your project actually needs.

Strengths Comparison

Fillamentum CPE Strengths

  • Better chemical resistance than PETG; holds up to alcohols, water, acids, and bases
  • Tough and ductile with strong impact resistance; bends where PLA would snap
  • Heat resistant to roughly 75°C plus UV resistance, so it survives outdoors
  • Low moisture uptake and minimal shrink/warp for an engineering material
  • Strong layer adhesion suits thin-walled models and parts under mechanical stress

ASA Strengths

  • Excellent UV resistance (outdoors indefinitely), tough, matte surface
  • Less warping than ABS; low viscosity enables very high speed printing
  • High heat tolerance (~boiling water range)

Considerations

Fillamentum CPE Caveats

  • Bonds hard to the build plate; the wrong sheet can be damaged on part removal
  • Around 275°C at the nozzle rules out PTFE-lined hotends
  • Less widely stocked and pricier than PETG for a modest step up in performance

ASA Caveats

  • Still off-gasses; enclosure/ventilation recommended
  • Can still warp; needs tuning

Frequently Asked Questions

What is the difference between Fillamentum CPE and ASA?
Fillamentum CPE prints at 275°C nozzle / 90°C bed (No enclosure, low moisture sensitivity). ASA prints at 220-275°C nozzle / 90-110°C bed (Recommended enclosure, moderate moisture sensitivity).
Is Fillamentum CPE or ASA stronger?
Our dataset does not include comparable tensile strength values for both. Qualitatively, Fillamentum CPE is suited to better chemical resistance than petg, while ASA is suited to excellent uv resistance (outdoors indefinitely).
Which prints at a higher temperature, Fillamentum CPE or ASA?
Fillamentum CPE prints at a higher temperature (275°C nozzle vs 220-275°C for ASA).
Is Fillamentum CPE or ASA better for beginners?
Fillamentum CPE is better for beginners: enclosure is no and moisture sensitivity is low, vs recommended enclosure and moderate moisture for ASA.
Should I use Fillamentum CPE or ASA for outdoor use?
For outdoor use, ASA is usually the better fit (Excellent UV resistance (outdoors indefinitely)). Choose Fillamentum CPE instead when better chemical resistance than petg.