Prusament PETG Magnetite 40% vs PETG

Compare Prusament PETG Magnetite 40% and PETG filaments side-by-side so you can pick the right one for your 3D printing project.

Prusament PETG Magnetite 40% vs PETG: Prusament PETG Magnetite 40% is known for general use, while PETG is known for tougher than pla. Prusament PETG Magnetite 40% is easier to print; Prusament PETG Magnetite 40% prints at higher nozzle temperatures (270°C vs 230-250°C). Choose Prusament PETG Magnetite 40% for general use, or PETG for tougher than pla.

Key differences at a glance

Property
Prusament PETG Magnetite 40%
PETG
Nozzle temp
270°C
230-250°C
Bed temp
100°C
70-90°C
Enclosure needed
No
Optional
Ease of printing
Easy
Moderate
Moisture sensitivity
low
moderate

Detailed Comparison

Property
Prusament PETG Magnetite 40%
PETG
Tier Rating
Tier null
Tier A
Family
Specialty
PETG
Nozzle Temp
270°C
230-250°C
Bed Temp
100°C
70-90°C
Enclosure
not needed
optional
Cooling
Moderate cooling; too much cooling can hurt layer adhesion
Moisture Sensitivity
low
moderate

Green marks the generally easier or more forgiving option in that row, based on tier, enclosure needs, and moisture sensitivity. It is not always the better choice for a specific job, so weigh it against what your project actually needs.

Strengths Comparison

Prusament PETG Magnetite 40% Strengths

    PETG Strengths

    • Tougher than PLA, higher temp tolerance, more durable in real-world use
    • Good clarity and low friction among easy-to-print materials

    Considerations

    Prusament PETG Magnetite 40% Caveats

      PETG Caveats

      • Overhangs/bridges sag; supports can be hard to remove
      • Absorbs water fairly quickly

      Frequently Asked Questions

      What is the difference between Prusament PETG Magnetite 40% and PETG?
      Prusament PETG Magnetite 40% prints at 270°C nozzle / 100°C bed (No enclosure, low moisture sensitivity). PETG prints at 230-250°C nozzle / 70-90°C bed (Optional enclosure, moderate moisture sensitivity).
      Is Prusament PETG Magnetite 40% or PETG stronger?
      Our dataset does not include comparable tensile strength values for both. Qualitatively, Prusament PETG Magnetite 40% is suited to , while PETG is suited to tougher than pla.
      Which prints at a higher temperature, Prusament PETG Magnetite 40% or PETG?
      Prusament PETG Magnetite 40% prints at a higher temperature (270°C nozzle vs 230-250°C for PETG).
      Is Prusament PETG Magnetite 40% or PETG better for beginners?
      Prusament PETG Magnetite 40% is better for beginners: enclosure is no and moisture sensitivity is low, vs optional enclosure and moderate moisture for PETG.
      Should I use Prusament PETG Magnetite 40% or PETG for tougher than pla?
      For tougher than pla, Prusament PETG Magnetite 40% is usually the better fit (). Choose PETG instead when tougher than pla.

      Other Popular Comparisons