Ultrafuse ABS vs PETG

Compare Ultrafuse ABS and PETG filaments side-by-side so you can pick the right one for your 3D printing project.

Ultrafuse ABS vs PETG: Ultrafuse ABS is known for fast printing, while PETG is known for tougher than pla. Ultrafuse ABS is easier to print; Ultrafuse ABS prints at higher nozzle temperatures (255°C vs 230-250°C). Choose Ultrafuse ABS for fast printing, or PETG for tougher than pla.

Key differences at a glance

Property
Ultrafuse ABS
PETG
Nozzle temp
255°C
230-250°C
Bed temp
100°C
70-90°C
Enclosure needed
No
Optional
Ease of printing
Easy
Moderate
Moisture sensitivity
low
moderate

Detailed Comparison

Property
Ultrafuse ABS
PETG
Tier Rating
Tier null
Tier A
Family
ABS
PETG
Nozzle Temp
255°C
230-250°C
Bed Temp
100°C
70-90°C
Enclosure
not needed
optional
Cooling
Moderate cooling; too much cooling can hurt layer adhesion
Moisture Sensitivity
low
moderate

Green marks the generally easier or more forgiving option in that row, based on tier, enclosure needs, and moisture sensitivity. It is not always the better choice for a specific job, so weigh it against what your project actually needs.

Strengths Comparison

Ultrafuse ABS Strengths

  • Fast printing, acetone soluble (weld/vapor smooth), cheap, tough, decent heat resistance
  • Good impact toughness for the price

PETG Strengths

  • Tougher than PLA, higher temp tolerance, more durable in real-world use
  • Good clarity and low friction among easy-to-print materials

Considerations

Ultrafuse ABS Caveats

  • Warps heavily
  • Strong fumes/off-gassing; enclosure plus ventilation recommended
  • Poor UV resistance; yellows and gets brittle outdoors (ASA is the better outdoor/UV choice)

PETG Caveats

  • Overhangs/bridges sag; supports can be hard to remove
  • Absorbs water fairly quickly

Frequently Asked Questions

What is the difference between Ultrafuse ABS and PETG?
Ultrafuse ABS prints at 255°C nozzle / 100°C bed (No enclosure, low moisture sensitivity). PETG prints at 230-250°C nozzle / 70-90°C bed (Optional enclosure, moderate moisture sensitivity).
Is Ultrafuse ABS or PETG stronger?
Our dataset does not include comparable tensile strength values for both. Qualitatively, Ultrafuse ABS is suited to fast printing, while PETG is suited to tougher than pla.
Which prints at a higher temperature, Ultrafuse ABS or PETG?
Ultrafuse ABS prints at a higher temperature (255°C nozzle vs 230-250°C for PETG).
Is Ultrafuse ABS or PETG better for beginners?
Ultrafuse ABS is better for beginners: enclosure is no and moisture sensitivity is low, vs optional enclosure and moderate moisture for PETG.
Should I use Ultrafuse ABS or PETG for high-temperature parts?
For high-temperature parts, Ultrafuse ABS is usually the better fit (Fast printing). Choose PETG instead when tougher than pla.