Ultrafuse PC-ABS-FR vs ASA

Compare Ultrafuse PC-ABS-FR and ASA filaments side-by-side so you can pick the right one for your 3D printing project.

Ultrafuse PC-ABS-FR vs ASA: Ultrafuse PC-ABS-FR is known for extremely stiff, while ASA is known for excellent uv resistance (outdoors indefinitely). Ultrafuse PC-ABS-FR is easier to print; Ultrafuse PC-ABS-FR prints at higher nozzle temperatures (275°C vs 220-275°C). Choose Ultrafuse PC-ABS-FR for extremely stiff, or ASA for excellent uv resistance (outdoors indefinitely).

Key differences at a glance

Property
Ultrafuse PC-ABS-FR
ASA
Nozzle temp
275°C
220-275°C
Bed temp
105°C
90-110°C
Enclosure needed
No
Recommended
Ease of printing
Easy
Moderate
Moisture sensitivity
low
moderate

Detailed Comparison

Property
Ultrafuse PC-ABS-FR
ASA
Tier Rating
Tier null
Tier A
Family
PC
ASA
Nozzle Temp
275°C
220-275°C
Bed Temp
105°C
90-110°C
Enclosure
not needed
recommended
Cooling
Low to moderate; avoid drafts
Moisture Sensitivity
low
moderate

Green marks the generally easier or more forgiving option in that row, based on tier, enclosure needs, and moisture sensitivity. It is not always the better choice for a specific job, so weigh it against what your project actually needs.

Strengths Comparison

Ultrafuse PC-ABS-FR Strengths

  • Extremely stiff; useful where flex must be minimal
  • Surprisingly affordable in some brands

ASA Strengths

  • Excellent UV resistance (outdoors indefinitely), tough, matte surface
  • Less warping than ABS; low viscosity enables very high speed printing
  • High heat tolerance (~boiling water range)

Considerations

Ultrafuse PC-ABS-FR Caveats

  • Feeding can be difficult unless spool is close/direct-fed

ASA Caveats

  • Still off-gasses; enclosure/ventilation recommended
  • Can still warp; needs tuning

Frequently Asked Questions

What is the difference between Ultrafuse PC-ABS-FR and ASA?
Ultrafuse PC-ABS-FR prints at 275°C nozzle / 105°C bed (No enclosure, low moisture sensitivity). ASA prints at 220-275°C nozzle / 90-110°C bed (Recommended enclosure, moderate moisture sensitivity).
Is Ultrafuse PC-ABS-FR or ASA stronger?
Our dataset does not include comparable tensile strength values for both. Qualitatively, Ultrafuse PC-ABS-FR is suited to extremely stiff, while ASA is suited to excellent uv resistance (outdoors indefinitely).
Which prints at a higher temperature, Ultrafuse PC-ABS-FR or ASA?
Ultrafuse PC-ABS-FR prints at a higher temperature (275°C nozzle vs 220-275°C for ASA).
Is Ultrafuse PC-ABS-FR or ASA better for beginners?
Ultrafuse PC-ABS-FR is better for beginners: enclosure is no and moisture sensitivity is low, vs recommended enclosure and moderate moisture for ASA.
Should I use Ultrafuse PC-ABS-FR or ASA for outdoor use?
For outdoor use, ASA is usually the better fit (Excellent UV resistance (outdoors indefinitely)). Choose Ultrafuse PC-ABS-FR instead when extremely stiff.

Other Popular Comparisons