Ultrafuse TPU-95A vs PETG

Compare Ultrafuse TPU-95A and PETG filaments side-by-side so you can pick the right one for your 3D printing project.

Ultrafuse TPU-95A vs PETG: Ultrafuse TPU-95A is known for excellent layer adhesion, while PETG is known for tougher than pla. Ultrafuse TPU-95A is easier to print; PETG prints at higher nozzle temperatures (230-250°C vs 225°C). Choose Ultrafuse TPU-95A for excellent layer adhesion, or PETG for tougher than pla.

Key differences at a glance

Property
Ultrafuse TPU-95A
PETG
Nozzle temp
225°C
230-250°C
Bed temp
40°C
70-90°C
Enclosure needed
No
Optional
Ease of printing
Easy
Moderate
Moisture sensitivity
low
moderate

Detailed Comparison

Property
Ultrafuse TPU-95A
PETG
Tier Rating
Tier null
Tier A
Family
Flexible
PETG
Nozzle Temp
225°C
230-250°C
Bed Temp
40°C
70-90°C
Enclosure
not needed
optional
Cooling
Moderate cooling; too much cooling can hurt layer adhesion
Moisture Sensitivity
low
moderate

Green marks the generally easier or more forgiving option in that row, based on tier, enclosure needs, and moisture sensitivity. It is not always the better choice for a specific job, so weigh it against what your project actually needs.

Strengths Comparison

Ultrafuse TPU-95A Strengths

  • Excellent layer adhesion; extremely impact resistant; highly durable
  • Great for combat robots, tactical/rough-use parts
  • Rubber-like parts (gaskets, grips, bumpers, wheels)

PETG Strengths

  • Tougher than PLA, higher temp tolerance, more durable in real-world use
  • Good clarity and low friction among easy-to-print materials

Considerations

Ultrafuse TPU-95A Caveats

  • Slow printing; retraction can cause jams (especially in Bowden setups)
  • Stringing is common
  • Very moisture sensitive; wet TPU prints poorly

PETG Caveats

  • Overhangs/bridges sag; supports can be hard to remove
  • Absorbs water fairly quickly

Frequently Asked Questions

What is the difference between Ultrafuse TPU-95A and PETG?
Ultrafuse TPU-95A prints at 225°C nozzle / 40°C bed (No enclosure, low moisture sensitivity). PETG prints at 230-250°C nozzle / 70-90°C bed (Optional enclosure, moderate moisture sensitivity).
Is Ultrafuse TPU-95A or PETG stronger?
Our dataset does not include comparable tensile strength values for both. Qualitatively, Ultrafuse TPU-95A is suited to excellent layer adhesion, while PETG is suited to tougher than pla.
Which prints at a higher temperature, Ultrafuse TPU-95A or PETG?
PETG prints at a higher temperature (230-250°C nozzle vs 225°C for Ultrafuse TPU-95A).
Is Ultrafuse TPU-95A or PETG better for beginners?
Ultrafuse TPU-95A is better for beginners: enclosure is no and moisture sensitivity is low, vs optional enclosure and moderate moisture for PETG.
Should I use Ultrafuse TPU-95A or PETG for flexible parts?
For flexible parts, Ultrafuse TPU-95A is usually the better fit (Excellent layer adhesion). Choose PETG instead when tougher than pla.

Other Popular Comparisons